J Korean Acad Prosthodont.  1998 Jun;36(3):514-523.

A STUDY ON THE WEAR OF DENTAL RESTORATIVE MATERIALS

Affiliations
  • 1Department of Prosthodontics, School of Dentistry, Wonkwang University, Korea.

Abstract

The purpose of this study was to compare the wear characteristics of Type III Gold Alloy (Degular C; Degussa AG), VMK 95 (Vita Zahnfabrik), Vitadur Alpha (Vita Zahnfabrik), IPS Empress (Ivoclar-Vivadent) and Targis (Ivoclar-Vivadent). Ten samples of each material were abraded against enamel of extracted incisors for 160,000 cycles on the wear machine. The depth of wear scars on enamel was analized with profilometer (Alpha-step 200; Tencor). And the wear of material specimen was determined with micrometer (PB-1B; Mitutoyo Co. Japan). The results obtained were as follows : 1. Type III gold alloy (2.47micrometer) and Targis (5.89micrometer) caused less wear of enamel specimens compared to VMK 95 (75.59micrometer), IPS Empress (78.60micrometer) and Vitadur Alpha (78.89micrometer) (p<0.05). 2. The wear of material specimen when opposing enamel was the lowest in type III gold alloy (3.0micrometer), followed by Targis (69.8micrometer), IPS Empress (148.4micrometer). VMK 95 (298.0micrometer) and Vitadur Alpha (300.8micrometer) exhibited the most severe wear against enamel (p<0.05).


MeSH Terms

Alloys
Cicatrix
Dental Enamel
Incisor
Alloys
Full Text Links
  • JKAP
Actions
Cited
CITED
export Copy
Close
Share
  • Twitter
  • Facebook
Similar articles
Copyright © 2024 by Korean Association of Medical Journal Editors. All rights reserved.     E-mail: koreamed@kamje.or.kr